5 Steps to Successful Preservation
Step 1 - Removal
To remove the hide use a sharp knife only to start and finish the job. Use your hands to pry and pull the hide off. Leave the tallow on the hide to help keep the skin soft.
Step 2 - Curing
Lay hide down flesh side up in a cool dry place. Spread 3-5 lbs. of table salt on the flesh side. Let sit for 3-4 days until a crust forms and noticeable weeping stops.  If a locker plant is processing it, be sure to request salting and that it be kept cool for you. DO NOT FREEZE.  (If Frozen, Thaw & Salt)

Step 3 - Packing  
Fold sides toward center and roll up hair side out, keeping salt on the hide.  Wrap in paper
and put in a cardboard box with your name, address, phone number and how you want it tanned : leather or hair-on.
DO NOT USE PLASTIC BAGS.
Lack of air circulation can cause rot.  If you have stretched and dried the hide, gently roll it into a loose cylinder to avoid cracking.


Step 4
- Shipping
Hides are accepted for leather tanning all year, for hair-on tanning from October 1 through
March 1.
CARRIER WILL DISCARD AND NOT DELIVER OR RETURN ANY PACKAGE SHOWING SIGNS OF BLOOD ON OR ABOUT THE PACKAGE.  W.B. PLACE WILL NOT BE HELD RESPONSIBLE FOR PACKAGES DEEMED UNDELIVERABLE BY UPS OR ANY OTHER CARRIER.  Include identification both inside and outside of package clearly labeled: "ATTN:MARKING ROOM".  

Send to:  W. B. Place            
              368 W. Sumner St.
               Hartford, WI   53027
Step 5 - Payment
We do not accept payments prior to billing. When your tanning is complete, the hide is measured and you are billed accordingly. Hides will be shipped when complete payment is received.  You may pay with check, money order, MasterCard, or Visa.

Hunter Hide Exchange Program (Call for pricing information)

Timing
It takes approximately 2 to 3 months to return your hide depending on the time of year we receive it.  Cow, elk, moose, and buffalo can take longer.

(NOTE:   Due to the scale of our production process, we cannot provide special handling of Individual hides. We suggest unusual or prize-winning hides be taken elsewhere)

Hides We Tan Into Leather
Deer, Elk, Moose, Buffalo, and Cow.
All deerskin and cowhide are tanned to a thickness suitable for use in our products.  Elk, moose, buffalo and cow may be sided (split from head to tail) so they can be placed safely through our tanning equipment.  This will mean that if you ship one cowhide, you will have two "sides" returned to you.


Hides We Tan with the Hair On
DEER ONLY
Hair-on tanning carries no guarantee for the outcome. The condition of the animal, how it was skinned, and how it was preserved are beyond our control and can affect the final result.  Tails are fragile and often come off during the tanning process.   We do not tan capes for taxidermy.

Step into the past in Authentic Buckskins!

 

Color of Tanned Leather
The tanned skins are returned to you with their natural color (pearl).   You may exchange your hide for colored hide at a $5.00 extra charge..
Are you a manufacturer in search of a source of tanned cow, deer or bison? 
Please contact our Sales Department at
(262) 673-4000

 

corner_top_left.gif (106 bytes) baige_pixel.gif (807 bytes) corner_top_right.gif (106 bytes)
corner_bot_left.gif (852 bytes) © 2003 img_copyrght.gif (1193 bytes) corner_bot_right.gif (852 bytes)